| Jacket Color | Off-white |
|---|---|
| Jacket Material | PVC |
| Capacitance | 75.459 pF/m | 23 pF/ft |
| dc Resistance, Outer Conductor | 0.58 ohms/kft | 1.903 ohms/km |
| Diameter Over Jacket | 15.367 mm | 0.605 in |
| Operating Temperature | -20 °C to +80 °C (-4 °F to +176 °F) |
| Flat Plate Crush Strength | 1.429 kg/mm | 80 lb/in |
| Dielectric Material | PE spline |
| Average Power, Inner Conductor Temperature | 100 °C | 212 °F |
| Jacket Spark Test Voltage (rms) | 5000 V |
| UL/ETL Certification | CATVP/CMP |
| Installation temperature | -5 °C to +60 °C (+23 °F to +140 °F) |
| Peak Power | 40 kW |
| Insulation Resistance | 100000 MOhms-km |
| Outer Conductor Material | Corrugated copper |
| Inner Conductor Material | Copper-clad aluminum wire |
| Minimum Bend Radius, multiple Bends | 127 mm | 5 in |
| Inductance | 0.19 µH/m | 0.058 µH/ft |
| Number of Bends, typical | 25 |
| Attenuation, Ambient Temperature | 20 °C | 68 °F |
| Flexibility | Standard |
| Power Attenuation | 2.32500004768371 |
| Number of Bends, minimum | 15 |
| Outer Conductor OD | 13.843 mm | 0.545 in |
| Average Power, Ambient Temperature | 40 °C | 104 °F |
| Fire Retardancy Test Method | CMP, NFPA 262/CATVP |
| Cable Impedance | 50 ohm ±2 ohm |
| dc Test Voltage | 4000 V |
| Operating Frequency Band | 1 " 8800 MHz |
| Nominal Size | 1/2 in |
| Product Type | Air coaxial cable |
| Bending Moment | 5.423 N-m | 4 ft lb |
| Tensile Strength | 113 kg | 249.122 lb |
| dc Resistance, Inner Conductor | 0.45 ohms/kft | 1.476 ohms/km |
| Pulse Reflection | 0.005 |
| Velocity | 0.88 |
| c(ETL)us Certification | CATVP/CMP |
| ISO 9001:2015 | Designed, manufactured and/or distributed under this quality management system |
| Storage Temperature | -20 °C to +85 °C (-4 °F to +185 °F) |
| Product Series | HL4-50A |
| Inner Conductor OD | 4.801 mm | 0.189 in |
| Package Quantity | 1000 |