| Process | Brazing |
|---|---|
| Standards | AWS A5.8 |
| Length (In.) | 36 |
| Dia. (In.) | 5/32 |
| Brazing Range (F) | 1,670 to 1,750 |
| Container | Box |
| Material | Bronze |
| Application | Brazing |
| Tensile Strength (PSI) | 71,000 |
| Item | Brazing Alloy |
| Package Quantity | 1 |
| Contents | 56% Copper |
| Container Size | 10 lb |
| AWS Classification | RBCuZn-C |
| Flux Application | Flux Not Required |
| Tensile Strength | 71 ksi |
| Compatible Chuck Size | 1,670 deg F |
| Joining Applications | Cast Iron to Cast Iron, Cast Iron to Copper, Cast Iron to Nickel, Cast Iron to Stainless Steel, Cast Iron to Steel, Copper to Nickel, Copper to Stainless Steel, Copper to Steel, Nickel to Nickel, Nickel to Stainless Steel, Nickel to Steel, Stainless Steel to Stainless Steel, Stainless Steel to Steel, Steel to Steel |
| Alloy Form | Rod |
| Elongation | 25% |
| Liquidus | 1,630 deg F |
| Solidus | 1,590 deg F |
| Overall Length | 36 in |
| Capacity Shingles | 1,750 deg F |
| Silver Content | 0 % |
| Container Type | Box |
| Yield Strength | 64 ksi |
| Alloy Type | Low-Fuming Bronze |
| Alloy Composition | 56% to 60% Copper, 0.8% to 1.1% Tin, 0.25% to 1.2% Iron, 0.01% to 0.5% Manganese, 0.05% Lead, 0.04% to 0.15% Silicon, 0.01% Aluminum, 0.5% Other, Balance Zinc |
| Series | RBCuZn-C |
| Overall Diameter | 5/32 in |
| Finish/Coating | Flux-Coated |
| Minimum Brazing Temperature | 1,670 deg F |
| Maximum Brazing Temperature | 1,750 deg F |
| Wire Rope Length | 36 in |
| Length | 36 in |
| Country of Origin (subject to change) | China |